New Products /back


GL-A500 | GL-A500 STEEL PLATE

2011年10月31日 by admin

GL-A500 STEEL PLATE

 
GL-A500 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
For more information in GL-A500 steel grade, please refer to the following:
 
 
 
 
GL-A500 Chemical composition heat analysis

Element
GL-A500 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
 
 
 
 
GL-A500 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
GL-A500
8-260
500
610-770
16
33J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV A500, BV A550

Tags: GL-A500 STEEL PLATE  GL-A500  

0 Comments, 0 Trackbacks