New Products /back


GL-A690 Steel Plate

2011年10月31日 by admin

GL-A690 Steel Plate

 
GL-A690 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in GL-A690.
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in GL-A690 steel grade, please refer to the following:

 
 
 
 
GL-A690 Chemical composition heat analysis

Element
GL-A690 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
 
 
 
 
GL-A690 Mechanical properties,                           longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
GL-A690
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV A690 | BV A420
 

Tags: GL-A690 Steel Plate  GL-A690  

0 Comments, 0 Trackbacks