GL-D460 | GL-D460 STEEL PLATE

2011年10月31日 by admin

GL-D460 STEEL PLATE

 
GL-D460 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting Extra high strength steel grade.

 
For more information in GL-D460 steel grade, please refer to the following:

 
 
 
GL-D460 Chemical composition heat analysis

Element
GL-D460 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
 
 
 
 
           
GL-D460 Mechanical properties,                           longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
GL-D460
8-260
460
570-720
17
31J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV D460 | BV D500