New Products /back


GL-D550 STEEL PLATE | GL-D550

2011年11月4日 by admin

GL-D550 STEEL PLATE

 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
 
For more information in GL-D550 steel grade, please refer to the following:

 
 
 
GL-D550 Chemical composition heat analysis

Element
GL-D550 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
         
 
 
 
GL-D550 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
GL-D550
8-260
550
670-830
16
37J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV D550 | BV D600

 

Tags: GL-D550  GL-D550 STEEL PLATE  

None Comments, None Trackbacks