GL-D690 Chemical composition heat analysis

Element
GL-D690 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
          
 
 
 
GL-D690 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
GL-D690
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 