GL DH32 GL grade dh32 dh32 steel plate

2011年4月5日 by admin

GL DH32,DH32,GL Grade DH32,GL-D32,DH32 steel grade

 

Adopt Standard: GL
Gang steel grade:

GL Grade

GL-D

GL-A

GL-B

GL-E

GL-A32

GL-D32

GL-E32

GL-F32

GL-A36

GL-D36

GL-E36

GL-F36

GL-A40

GL-D40

GL-E40

GL-F40

 GL

GL

GL

 

GL DH32 steel grade for shipbuilding material.

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL DH32 Z15, GL DH32 Z25, GL DH32 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.

 

Gangsteel exported GL DH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About GL DH32 detail information, please refer to technical date in following.

 

GL DH32 Chemical composition heat analysis

 

Element

GL DH32  Max %

Element

GL DH32 max %

C

0.18

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.035

CR

0.20

P

0.035

Ni

0.40

ALs

    0.015 MIN

MO

0.08

    NB

  0.02-0.05

N

 

           

 

GL DH32 Mechanical properties,            longitudinal min impact energy

 

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

GL DH32

8-200

315

440-590

22

31J

 

If you have any need in GL DH32 steel plate, please feel free to contact us soon to get a competitive price.

 

 