New Products /back


GL D40 GL DH40 GL Grade DH40 steel plate

2011年4月5日 by admin

GL DH40,DH40,GL Grade DH40,GL-D40,DH40 steel grade

 

Adopt Standard: GL
Gang steel grade:

GL Grade

GL-D

GL-A

GL-B

GL-E

GL-A32

GL-D32

GL-E32

GL-F32

GL-A36

GL-D36

GL-E36

GL-F36

GL-A40

GL-D40

GL-E40

GL-F40

DNV

BV

LR

ABS

RINA

NK

KR

 

GL Grade DH40 steel plate

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL DH40 Z15, GL DH40 Z25, GL DH40 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond DNV,CCS,ABS,GL,BV,LR,KR,RINA,NK classification society approval.

We sincerely hope old and new customers to visit our mill for a long steel business

 

About GL DH40 Grade detail information, please refer to technical date in following.

 

GL DH40 Chemical composition heat analysis

Element

GL DH40  Max %

Element

GL DH40 max %

C

0.18

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.035

CR

0.20

P

0.035

Ni

0.40

ALs

    0.015 MIN

 Mo

0.08

    NB

  0.02-0.05

N

 

            

 

GL DH40 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

GL DH40

8-200

390

510-650

20

41J

 

If you have any need in GL DH40 steel plate, please feel free to contact us soon to get a competitive price.

 

 

Tags: GL D40  GL DH40  GL Grade DH40  DH40  