GL-E420 | GL-E420 steel plate
2011年11月4日 by admin
GL-E420 steel plate
GL-E420 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in GL E690.
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.
For more information in GL-E420 steel grade, please refer to the following:
GL-E420 Chemical composition heat analysis
Element | GL-E420 Max % |
C | 0.20 |
Mn | 1.70 |
Si | 0.55 |
S | 0.030 |
P | 0.030 |
N | 0.020 |
Other alloy elements should be along with GL Society Classification requirement.
GL-E420 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -40 degree | |
GL-E420 | 8-260 | 420 | 530-680 | 18 | 28J |
Note: the impact energy under less 150mm thickness
Related Grade: NV E420 | BV E460