GL-F460 Chemical composition heat analysis
Element | GL-F460 Max % |
C | 0.18 |
Mn | 1.70 |
Si | 0.55 |
S | 0.025 |
P | 0.025 |
N | 0.020 |
Other alloy elements should be along with GL Society Classification requirement.
GL-F460 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -60 degree | |
GL-F460 | 8-260 | 460 | 570-720 | 17 | 31J |
Note: the impact energy under less 150mm thickness