FH36 GL F36 GL FH36 GL Grade FH36 steel plate

2011年4月5日 by admin

GL FH36,FH36,GL Grade FH36,GL-F36,FH36 steel grade

 

Adopt Standard: GL
Gang steel grade:

GL Grade

GL-D

GL-A

GL-B

GL-E

GL-A32

GL-D32

GL-E32

GL-F32

GL-A36

GL-D36

GL-E36

GL-F36

GL-A40

GL-D40

GL-E40

GL-F40

DNV

BV

LR

ABS

RINA

NK

KR

 

GL Grade FH36 steel plate

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL FH36 Z15, GL FH36 Z25, GL FH36 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.

 

Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We export

FH36 steel material directly in our mill cost price from sales department. Certificate Test in

EN10204-3.2

 

We sincerely hope old and new customers to visit our mill for a long steel business

About GL FH36 detail information, please refer to technical date in following.

 

GL FH36 Chemical composition heat analysis

Element

GL FH36  Max %

Element

GL FH36 max %

C

0.16

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.025

CR

0.20

P

0.025

Ni

0.80

ALs

    0.015 MIN

 Mo

0.08

    NB

  0.02-0.05

N

0.009

           

GL FH36 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-60 degree

GL FH36

8-200

355

490-620

21

34J

 

If you have any need in GL FH36 steel plate, please feel free to contact us soon to get a competitive price.

 

 