FH40 GL FH40 GL F40 GL Grade Fh40 steel plate

2011年4月5日 by admin

GL FH40,FH40,GL Grade FH40,GL-F40,FH40 steel grade

 

Adopt Standard: GL
Gang steel grade:

GL Grade

GL-D

GL-A

GL-B

GL-E

GL-A32

GL-D32

GL-E32

GL-F32

GL-A36

GL-D36

GL-E36

GL-F36

GL-A40

GL-D40

GL-E40

GL-F40

DNV

BV

LR

ABS

RINA

NK

KR

 

GL Grade FH40 steel plate

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL FH40 Z15, GL FH40 Z25, GL FH40 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond DNV,CCS,ABS,GL,BV,LR,KR,RINA,NK classification society approval.

We sincerely hope old and new customers to visit our mill for a long steel business

 

About GL FH40 Grade detail information, please refer to technical date in following.

 

GL FH40 Chemical composition heat analysis

Element

GL FH40  Max %

Element

GL FH40 max %

C

0.16

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.025

CR

0.20

P

0.025

Ni

0.80

ALs

    0.015 MIN

 Mo

0.08

    NB

  0.02-0.05

N

0.009

           

 

GL FH40 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-60 degree

GL FH40

8-200

390

510-650

20

41J

 

If you have any need in GL FH40 steel plate, please feel free to contact us soon to get a competitive price.

 

 

Tags: GL FH40  FH40  GL  GL grade FH40  gl f40  