304L Stainless plate,A240 304L stainless steel plate,ASTM A240 304L
2013年11月22日 by admin
ASTM A240 standard specification for chromium and chromium-nnickel stainless steel plate, sheet, and strip for pressure vessels and for general applications
Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2
Gangsteel is specialized in supplyingASTM A240 steel plate inA240 Grade 304L. For more information of 304L stainless steel plates, please check them in following:
ASTM A240 Grade 304LChemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Mn | P | S | Si | Cr | Ni | |
ASTM A240 Grade 304L | 0.03 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 | 8.0-12.0 |
Mo | N | Cu | | | | | |
| 0.10 | | | | | |
Grade | ASTM A240 Grade 304LMechanical Property | ||||
Yield | Tensile | Elongation | Hardness, max | ||
ASTM A240 Grade 304L | Min Mpa | Mpa | Min % | Brinell | Rockwell B |
170 | 485 | 40% | 201 | 92 |
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
If you need more stock steel plates in pressure vessel steel plate, please click warehouse sizes.
Related Grade:A240 Grade 304| A240 Grade 316| A240 Grade 316l| A240 Grade 310 | A240 Grade 304H| A240 Grade 321| A240 Grade 316H