A240 304 Stainless steel plate,SS304 stainless plate

2013年11月22日 by admin

 

ASTM A240 Grade 304| SS304 STAINLESS
 
ASTM A240 standard specification for chromium and chromium-nnickel stainless steel plate, sheet, and strip for pressure vessels and for general applications
 
Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2

Gangsteel is specialized in supplyingASTM A240 steel plate inA240 Grade 304. For more information of 304 stainless steel plates, please check them in following:
 

  ASTM A240 Grade 304Chemical Composition
Grade
The Element Max (%)
C
Mn
P
S
Si
Cr
Ni
ASTM A240 Grade 304
0.08
2.00
0.045
0.030
0.75
18.0-20.0
8.0-10.5
Mo
N
Cu
 
 
 
 
 
0.10
 
 
 
 
 

 
 

Grade
ASTM A240 Grade 304Mechanical Property
Yield
Tensile
Elongation
Hardness, max
ASTM A240 Grade 304
Min Mpa
Mpa
Min %
Brinell
Rockwell B
205
515
40%
201
92

 
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
 
If you need more stock steel plates in pressure vessel steel plate, please click warehouse sizes.
 
Related Grade:A240 Grade 304L| A240 Grade 316| A240 Grade 316l| A240 Grade 310 | A240 Grade 304H| A240 Grade 321| A240 Grade 316H
 
 
 
 

Tags: A240 304  304 Stainless steel plate  SS304 stainless plate  SS304  

0 Comments, 0 Trackbacks