New Products /back


316L,ASTM A240 Grade 316L|,SS316L STAINLESS

2013年10月14日 by admin

 

ASTM A240 Grade 316L| SS316L STAINLESS
 
ASTM A240 standard specification for chromium and chromium-nnickel stainless steel plate, sheet, and strip for pressure vessels and for general applications
 
Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2

Gangsteel is specialized in supplyingASTM A240 steel plate inA240 Grade 316L. For more information of 316L stainless steel plates, please check them in following:
 

  ASTM A240 Grade 316LChemical Composition
Grade
The Element Max (%)
C
Mn
P
S
Si
Cr
Ni
ASTM A240 Grade 316L
0.03
2.00
0.045
0.030
0.75
16.0-18.0
10.0-14.0
Mo
N
Cu
 
 
 
 
2.00-3.00
0.10
 
 
 
 
 

 
 

Grade
ASTM A240 Grade 316LMechanical Property
Yield
Tensile
Elongation
Hardness, max
ASTM A240 Grade 316L
Min Mpa
Mpa
Min %
Brinell
Rockwell B
170
485
40%
217
95

 
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
 
If you need more stock steel plates in pressure vessel steel plate, please click warehouse sizes.
 
Related Grade:A240 Grade 304| A240 Grade 304L| A240 Grade 316l| A240 Grade 310 | A240 Grade 304H| A240 Grade 321| A240 Grade 316H
 
 
 
 

Tags: 316L  ASTM A240 Grade 316L  SS316L STAINLESS  

0 Comments, 0 Trackbacks