New Products /back


321 Stainless plate,A240 321,ASTM A240 321 Sainless steel plate

2013年11月22日 by admin

 

ASTM A240 Grade 321| SS321 STAINLESS
 
ASTM A240 standard specification for chromium and chromium-nnickel stainless steel plate, sheet, and strip for pressure vessels and for general applications
 
Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2

Gangsteel is specialized in supplyingASTM A240 steel plate inA240 Grade 321. For more information of 321 stainless steel plates, please check them in following:
 

  ASTM A240 Grade 321Chemical Composition
Grade
The Element Max (%)
C
Mn
P
S
Si
Cr
Ni
ASTM A240 Grade 321
0.08
2.00
0.045
0.030
0.75
17.0-19.0
9.0-12.0
Mo
N
Cu
 
 
 
 
 
0.1
Ti5X(C+N)
 
 
 
 

 
 

Grade
ASTM A240 Grade 321Mechanical Property
Yield
Tensile
Elongation
Hardness, max
ASTM A240 Grade 321
Min Mpa
Mpa
Min %
Brinell
Rockwell B
205
515
40%
217
95

 
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
 
If you need more stock steel plates in pressure vessel steel plate, please click warehouse sizes.
 
Related Grade:A240 Grade 304| A240 Grade 304L| A240 Grade 316| A240 Grade 316H| A240 Grade 304H| A240 Grade 321| A240 Grade 316L
 
 
 
 

Tags: 321  321 Stainless plate  A240 321  ASTM A240 321 Sainless steel plate  

0 Comments, 0 Trackbacks