AB/EQ47|ABS EQ47 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ47. For more information of Grade EQ47 steel plate, please check them in following:
AB/EQ47 Extra high Strength Chemical Composition in Tempering and Quenching | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
AB/EQ47 | 0.20 | 0.55 | 1.7 | 0.035 | 0.035 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/EQ47 Extra high strength property in tempering and quenching | ||||||
Grade | Mechanical Property | Charpy V Impact Test | ||||
Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
Min Mpa | Mpa | Min % | -40 | J | J | |
AB/EQ47 | 460 | 570-720 | 17 | 31 | 46 | |
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/EQ47 | |||||||
NV E460 | GL-E460 | LR/EH46 | BV/E460 | CCS/E460 | K E47 | R E47 | RI/E460 |
To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.
Tags: ABS EQ41 AB/EQ47 ABS Grade EQ47 ABS Gr EQ47 AB/EQ47 steel plate EQ47 steel grade