AB/FQ70|ABS FQ70 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade FQ70. For more information of Grade FQ70 steel plate, please check them in following:
AB/FQ70 Extra high Strength Chemical Composition in Tempering and Quenching | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
AB/FQ70 | 0.18 | 0.55 | 1.60 | 0.025 | 0.025 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/FQ70 Extra high strength property in tempering and quenching | ||||||
Grade | Mechanical Property | Charpy V Impact Test | ||||
Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
Min Mpa | Mpa | Min % | -60 | J | J | |
AB/FQ70 | 690 | 770-940 | 14 | 41 | 62 | |
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/FQ70 | |||||||
NV F690 | GL-F690 | LR/FH69 | BV/F690 | CCS/F690 | K F70 | R F70 | RI/F690 |
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.