Gangsteel is specialized in supplying ABS general strength steel plate in ABS Grade B. For more information of Grade B steel plate, please check them in following:

 

 

ABS GRADE B  general strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

N

ABS GRADE B

0.21

0.35

0.80

0.035

0.035

0.02

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

ABS GRADE B high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

ABS GRADE B

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

235

400-520

18%

20

27

50t≤70

235

400-520

18%

24

34

70t≤100

235

400-520

18%

27

41

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of ABS GRADE B

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV B

GL-B

LR/B

BV/B

CCS/B

K B

R B

RI/B

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

Tags: ABS B  AB/ B  ABS Grade B  ABS Gr B  AB/ B steel plate  ABS Grade B supplier  

0 Comments, 0 Trackbacks