New Products /back


SM490B SM490B steel SM490B Grade

2011年3月31日 by admin

SM490B,SM490B steel,SM490B Grade,SM490B steel grade,SM490B steel plate,SM490B

 

Adopt standard: JIS G3106-2004

Grade:SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,SM490C,SM490B,SM400A,SM400B,SM400C,SM490A steel grade.

 

SM490B Steel Plate

SM490A, SM490B and SM490C steel grade is a low carbon, welding structural steel. With this low carbon equivalent, it process good cold forming property. SM490A, SM490B and SM490C  steel plates usual supplied in Hot rolled or control rolled delivery condition.


SM490A,SM490B and SM490C are different in carbon element. Others are the same. SM490C carbon is 0.18%, SM490B is 0.18-0.20% and SM490A is 0.20-0.22%.

The equal steel grade is JIS SM570, A572 Gr.50, EN S355JR, ST 52-3 and so on

 

Gangsteel exported SM490B to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM490B, Please contact Gangsteel to get the competitive price soon.

 

SM490B steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.18
0.20

Product Analysis

1.60

 

Product Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

SM490B steel grade Tensile Requirements

 

Mechanical Property of SM490B steel grade

SM490B steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm
Elongation under in [16 mm], min, %
Elongation above in [16 mm], min, %

Tensile strength, kis [MPa]

[490-610]

Yield strength, min, kis [MPa]

[325]

[315]

[295]

[325]

[285]

17

23

 

Gangsteel had many stocks in alloy steel of SM490B steel plates. If you need them more stock, please click Gangsteel stock.

 

For more information in Price and MTC in SM490B steel grade, please contact us by email or calling.

 

SM490B,SM490B steel,SM490B Grade,SM490B steel grade,SM490B steel plate,SM490B

 

Tags: SM490B  SM490B steel  SM490B Grade  