New Products /back


SM490YA,SM490YA steel,SM490YA Grade,SM490YA steel grade,SM490YA steel plate

2011年3月31日 by admin

SM490YA,SM490YA steel,SM490YA Grade,SM490YA steel grade,SM490YA steel plate

 

Adopt standard: JIS G3106-2004

Grade:SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,SM490C,SM490B,SM400A,SM400B,SM400C,SM490A steel grade.

 

SM490YA Steel Plate

 

SM490YA steel plates usual supplied in normalized or control rolled delivery condition. SM490YA steel grade is a low carbon, high strength structural steel With this low carbon equivalent, it process good cold forming property.


SM490YA steel grade usual be used in machinery parts, boom, crane, chassis , buildings bridges and mobile equipment.

 

Gangsteel exported SM490YA to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM490YA, Please contact Gangsteel to get the competitive price soon.

 

SM490YA steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.20
0.20

Product Analysis

1.60

 

Product Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

 

SM490YA steel grade Tensile Requirements

 

Mechanical Property of SM490YA steel grade

SM490YA steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm
Elongation under in [16 mm], min, %
Elongation in above [16 mm], min, %

Tensile strength, kis [MPa]

[490-610]

Yield strength, min, kis [MPa]

[365]

[355]

[355]

[325]

[…]

15

21

 

Gangsteel had many stocks in alloy steel of SM490YA steel plates. If you need them more stock, please click Gangsteel stock.

For more information in Price and MTC in SM490YA steel grade, please contact us by email or calling.

 

SM490YA,SM490YA steel,SM490YA Grade,SM490YA steel grade,SM490YA steel plate

 

 

Tags: SM490YA  SM490YA steel  SM490YA Grade  