New Products /back


SM520B,SM520B steel,SM520B Grade

2011年3月31日 by admin

SM520B,SM520B steel,SM520B Grade,SM520B steel grade,SM520B steel plate,SM520B grade

 

Adopt standard: JIS G3106-2004

Grade:SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,SM490C,SM490B,SM400A,SM400B,SM400C,SM490A steel grade.

 

SM520B Steel Plate

 

SM520B steel grade is a low carbon, high strength structural steel With this low carbon equivalent, it process good cold forming property. SM520B steel plates usual supplied in normalized or control rolled delivery condition.


SM520B steel grade usual be used in machinery parts, boom, crane, chassis , buildings bridges and mobile equipment.

 

Gangsteel exported SM520B to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM520B, Please contact Gangsteel to get the competitive price soon.

 

SM520B steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.20
0.20

Product Analysis

1.60

 

Product Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

 

SM520B steel grade Tensile Requirements

 

Mechanical Property of SM520B steel grade

SM520B steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm

Elongation under in [16 mm], min, %
Elongation in above [16 mm], min, %

Tensile strength, kis [MPa]

[520-640]

Yield strength, min, kis [MPa]

[365]

[355]

[355]

[325]

[…]

15

21

 

Gangsteel had many stocks in alloy steel of SM520B steel plates. If you need them more stock, please click Gangsteel stock.

For more information in Price and MTC in SM520B steel grade, please contact us by email or calling.

 

SM520B,SM520B steel,SM520B Grade,SM520B steel grade,SM520B steel plate,SM520B grade

 

 

Tags: SM520B  SM520B steel  SM520B Grade  

0 Comments, 0 Trackbacks