New Products /back


SM570,SM570 steel,SM570 Grade,SM570 steel plate

2011年4月14日 by admin

SM570,SM570 steel,SM570 Grade,SM570 steel grade,SM570 steel plate,SM570 material

 

Adopt standard: JIS G3106-2004

Grade:SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,SM490C,SM490B,
SM400A,SM400B,SM400C,SM490A steel grade.

 

SM570 Steel Plate

 

SM570 steel grade is a low carbon, high strength structural steel With this low carbon equivalent, it process good cold forming property. SM570 and SM520 steel plates usual supplied in normalized or control rolled delivery condition.


SM570 and SM520 steel grade usual be used in machinery parts, boom, crane, chassis , buildings bridges and mobile equipment.The equal steel grade is ST52-3, A572 Gr.50, EN S355JR and so on

 

Gangsteel exported SM570 to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM570 and SM520, Please contact Gangsteel to get the competitive price soon.

 

SM570 steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon,
max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.18
0.18

Product Analysis

1.60

 

Product

Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

SM570 steel grade Tensile Requirements

 

Mechanical Property of SM570 steel grade

SM570 steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm

Elongation under in [16 mm], min, %
Elongation in above [16 mm], min, %

Tensile strength, kis [MPa]

[570-720]

Yield strength, min, kis [MPa]

[460]

[450]

[430]

[420]

[…]

19

20

 

Gangsteel had many stocks in alloy steel of SM570 and SM520 steel plates. If you need them more stock, please click Gangsteel stock.

For more information in Price and MTC in SM570 and SM520 steel grade , please contact us by email or calling.

 

SM570,SM570 steel,SM570 Grade,SM570 steel grade,SM570 steel plate,SM570 material

 

 

grade,SM570 steel plate,SM570 material

 

 

Adopt standard: JIS G3106-2004

Grade:SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,SM490C,SM490B,
SM400A,SM400B,SM400C,SM490A steel grade.

 

SM570 Steel Plate

 

SM570 steel grade is a low carbon, high strength structural steel With this low carbon equivalent, it process good cold forming property. SM570 and SM520 steel plates usual supplied in normalized or control rolled delivery condition.


SM570 and SM520 steel grade usual be used in machinery parts, boom, crane, chassis , buildings bridges and mobile equipment.The equal steel grade is ST52-3, A572 Gr.50, EN S355JR and so on

 

Gangsteel exported SM570 to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM570 and SM520, Please contact Gangsteel to get the competitive price soon.

 

SM570 steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon,
max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.18
0.18

Product Analysis

1.60

 

Product

Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

SM570 steel grade Tensile Requirements

 

Mechanical Property of SM570 steel grade

SM570 steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm

Elongation under in [16 mm], min, %
Elongation in above [16 mm], min, %

Tensile strength, kis [MPa]

[570-720]

Yield strength, min, kis [MPa]

[460]

[450]

[430]

[420]

[…]

19

20

 

Gangsteel had many stocks in alloy steel of SM570 and SM520 steel plates. If you need them more stock, please click Gangsteel stock.

For more information in Price and MTC in SM570 and SM520 steel grade , please contact us by email or calling.

 

SM570,SM570 steel,SM570 Grade,SM570 steel grade,SM570 steel plate,SM570 material

 

 

 

Tags: SM570  SM570 steel  SM570 Grade  SM570 steel grade  SM570 steel plate  SM570 material  

0 Comments, 0 Trackbacks