SPV315 steel plate is for pressure vessels for intermediate temperature service in JIS G3115-2000
SPV315 Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

About the detail information of SPV315 is in the following.


SPV315 Chemical composition cast analysis:

Element

SPV315  Max %

C

0.18

Si

0.15-0.55

Mn

1.60

P

0.030

S

0.030

 

SPV315 Mechanical properties:              

Grade

Thickness

Yield Strength

Tensile Strength

(mm)

MPa (min)

MPa

 

 

 

SPV315

≤ 50

315

490-610

50> to ≤100

295

490-610

100> to ≤200

275

490-610

 