KR AH47 Chemical composition heat analysis

Element
KR AH47 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with KR Society Classification requirement.
           
 
 
 
 
KR AH47 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
KR AH47
8-260
460
570-720
17
31J