LR DH27S steel grade

DH27S steel grade specification:
Thickness: 6mm to 200mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

 

Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.

 

Gangsteel exported LR DH27S steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About LR DH27S detail information, please refer to technical date in following:

 

LR DH27S Chemical composition heat analysis

Element

LR DH27S Max %

Element

LR DH27S max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

  0.015 min

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.03-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

LR DH27S Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

LR DH27S

8-200

265

400-530

22

27

Note: the impact energy under less 50mm thickness

 

If you have any need in LR DH27S steel plate, please feel free to contact us soon to get a competitive price.

 