LR AH27S Steel Grade, LR/AH27S,LR AH27S,LR Grade AH27S
2011年3月29日 by admin
LR AH27S Steel Grade, LR/AH27S,LR AH27S,LR Grade AH27S
Adopt Standard: LR
LR steel grade:
LR/A | LR/B | LR/E | LR/D |
LR/AH36 | LR/DH36 | LR/EH36 | LR/FH36 |
LR/AH32 | LR/DH32 | LR/EH32 | LR/FH32 |
LR/AH40 | LR/DH40 | LR/EH40 | LR/FH40 |
LR/AH27S | LR/DH27S | LR/EH27S | LR/FH27S |
BV | ABS | DNV | GL |
LR AH27S steel grade
AH27S steel grade specification:
Thickness: 6mm to 200mm,
Width: 1500mm to 4020mm
Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.
Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.
Gangsteel exported LR AH27S steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.
We sincerely hope old and new customers to visit our mill for a long steel business
About LR AH27S detail information, please refer to technical date in following:
LR AH27S Chemical composition heat analysis
Element | LR AH27S Max % | Element | LR AH27S max % |
C | 0.18 | Ni | 0.40 |
Mn | 0.90-1.60 | Mo | 0.08 |
Si | 0.50 | Al | 0.015 min |
S | 0.035 | Nb | 0.20-0.05 |
P | 0.035 | V | 0.03-0.10 |
Cu | 0.35 | Ti | 0.02 |
Cr | 0.20 | N | |
LR AH27S Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | 0 degree | |
LR AH27S | 8-200 | 265 | 400-530 | 22 | 27 |
Note: the impact energy under less 50mm thickness