LR AH36 Steel Grade, LR/AH36,LR AH36,LR Grade AH36

2011年3月29日 by admin

LR AH36 Steel Grade, LR/AH36,LR AH36,LR Grade AH36,

 

Adopt Standard: LR

LR steel grade:

LR/A

LR/B

LR/E

LR/D

LR/AH36

LR/DH36

LR/EH36

LR/FH36

LR/AH32

LR/DH32

LR/EH32

LR/FH32

LR/AH40

LR/DH40

LR/EH40

LR/FH40

LR/AH27S

LR/DH27S

LR/EH27S

LR/FH27S

BV

ABS

DNV

GL

 

LR AH36 steel grade

AH36 steel grade specification:
Thickness: 6mm to 200mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, LR EH32 Z15, LR EH32 Z25, LR EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

 

Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.

 

Gangsteel exported LR AH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About LR AH36 detail information, please refer to technical date in following:

 

LR AH36 Chemical composition heat analysis

Element

LR AH36 Max %

Element

LR AH36 max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

  0.015 min

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.03-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

LR AH36 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

0 degree

LR AH36

8-200

355

490-620

21

34J

Note: the impact energy under less 50mm thickness

 

If you have any need in LR AH36 steel plate, please feel free to contact us soon to get a competitive price.

 

Tags: LR AH36  LR Grade AH36  AH36 Steel Grade  