New Products /back


DH32,LR/DH32,LR DH32,DH32 steel,LR/DH32 steel,LR DH32 steel,steel plate,LR

2011年3月9日 by admin

 

DH32,LR/DH32,LR DH32,DH32 steel,LR/DH32 steel,LR DH32 steel,steel plate,LR
 
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade LR/AH36, LR/DH36, LR/EH36, LR/FH36, LR/AH32, LR/DH32, LR/EH32, LR/FH32, LR GRADE A, LR GRADE B, LR GRADE D, LR GRADE E. LR/AH40, LR/DH40, LR/EH40, LR/FH40.
 
 
In usual if DH32 steel plate thickness above 40mm, mill request the normalized in hot rolled plate, if above 150mm thickness our mill also could use the electroslag remelting technical to do for our customers.
DH32 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:

Thickness: 6mm to 240mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.
 
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

We sincerely hope old and new customers to visit our mill for a long steel business
 
About DH32 detail information,please refer to technical date in following.
 
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 DH32
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
DH32
8mm-50mm
Min 315Mpa
440-590Mpa
22%
-20
 34J
51mm-70mm
Min 315Mpa
440-590Mpa
22%
-20
 38J
71mm-100mm
Min 315Mpa
440-590Mpa
22%
-20
 46J
The min impact energy is longitudinal energy

 
 
If you have any need in DH32 steel plate, please feel free to contact us soon.
 
 
 

Tags: DH32  LR/DH32  LR DH32  DH32 steel  LR/DH32 steel  LR DH32 steel  steel plate  LR  

None Comments, None Trackbacks