New Products /back


DH36,LR/DH36,LR DH36,DH36 steel,LR/DH36 steel,LR DH36 steel,LR,ship steel plate

2011年3月9日 by admin

 

DH36,LR/DH36,LR DH36,DH36 steel,LR/DH36 steel,LR DH36 steel,LR,ship steel plate
 
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade LR/AH36, LR/DH36, LR/EH36, LR/FH36, LR/AH32, LR/DH32, LR/EH32, LR/FH32, LR GRADE A, LR GRADE B, LR GRADE D, LR GRADE E. LR/AH40, LR/DH40, LR/EH40, LR/FH40.
 
 
 
DH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:

Thickness: 6mm to 180mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
Henan Gang iron and steel co., Ltd also could supply super thickness plate which beyond nine classification society approval.
 
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

 
Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for long steel business
 
About DH36 detail information,please refer to technical date in following.
 
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 DH36
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
DH36
8mm-50mm
Min 355Mpa
490-620Mpa
21%
-20
 34J
51mm-70mm
Min 355Mpa
490-620Mpa
21%
-20
 41J
71mm-100mm
Min 355Mpa
490-620Mpa
21%
-20
 50J
The min impact energy is longitudinal energy

 
 
Our mill DH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in DH36 steel plate, please feel free to contact us soon.
 
 
 

Tags: DH36  LR/DH36  LR DH36  DH36 Steel  LR/DH36 steel  LR DH36 steel  LR  Ship steel plate  

0 Comments, 0 Trackbacks