LR DH36 steel grade

DH36 steel grade specification:
Thickness: 6mm to 200mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

 

Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.

 

Gangsteel exported LR DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About LR DH36 detail information, please refer to technical date in following:

 

LR DH36 Chemical composition heat analysis

Element

LR DH36 Max %

Element

LR DH36 max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

  0.015 min

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.03-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

LR DH36 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

LR DH36

8-200

355

490-620

21

34J

Note: the impact energy under less 50mm thickness

 