LR EH36 Grade, LR/EH36,LR EH36,LR Grade EH36,
2011年3月29日 by admin
LR EH36 Steel Grade, LR/EH36,LR EH36,LR Grade EH36,
Adopt Standard: LR
LR steel grade:
LR/A | LR/B | LR/E | LR/D |
LR/AH36 | LR/DH36 | LR/EH36 | LR/FH36 |
LR/AH32 | LR/DH32 | LR/EH32 | LR/FH32 |
LR/AH40 | LR/DH40 | LR/EH40 | LR/FH40 |
LR/AH27S | LR/DH27S | LR/EH27S | LR/FH27S |
BV | ABS | DNV | GL |
LR EH36 steel grade
EH36 steel grade specification:
Thickness: 6mm to 200mm,
Width: 1500mm to 4020mm
Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.
Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.
Gangsteel exported LR EH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.
We sincerely hope old and new customers to visit our mill for a long steel business
About LR EH36 detail information, please refer to technical date in following:
LR EH36 Chemical composition heat analysis
Element | LR EH36 Max % | Element | LR EH36 max % |
C | 0.18 | Ni | 0.40 |
Mn | 0.90-1.60 | Mo | 0.08 |
Si | 0.50 | Al | 0.015 min |
S | 0.035 | Nb | 0.20-0.05 |
P | 0.035 | V | 0.03-0.10 |
Cu | 0.35 | Ti | 0.02 |
Cr | 0.20 | N | |
LR EH36 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -40 degree | |
LR EH36 | 8-200 | 355 | 490-620 | 21 | 34J |
Note: the impact energy under less 50mm thickness
If you have any need in LR EH36 steel plate, please feel free to contact us soon to get a competitive price.
Tags: LR EH36 Grade EH36 LR Grade EH36