New Products /back


FH36,LR/FH36,LR FH36,FH36 steel,LR FH36 steel,LR/FH36 steel,LR, FH36 steel plate

2011年3月9日 by admin

 

FH36,LR/FH36,LR FH36,FH36 steel,LR FH36 steel,LR/FH36 steel,LR, FH36 steel plate
 
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade LR/AH36, LR/DH36, LR/EH36, LR/FH36, LR/AH32, LR/DH32, LR/EH32, LR/FH32, LR GRADE A, LR GRADE B, LR GRADE D, LR GRADE E. LR/AH40, LR/DH40, LR/EH40, LR/FH40.
 
 
 
FH36 is a high strength ship steel grade, in -60 charpy V impact and normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.
 
Henan Gang iron and steel co., Ltd keeps a long cooperation with nine classification society to let them approval super thickness plates in our mill test certificate.
 
Henan Gang iron and steel co., Ltd had produced thickness is 110mm in this grade.
 
Henan Gang iron and steel co., Ltd supply FH36 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
 
About FH36 detail information,please check technical date in following.
 
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
FH36
0.160
0.10-0.5
0.9-1.6
0.025
0.025
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.350
0.080
0.02-0.05
0.080
0.020
0.012
 
 

 
 
 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
FH36
8mm-50mm
Min 355Mpa
490-620Mpa
21%
-60
 34J
51mm-70mm
Min 355Mpa
490-620Mpa
21%
-60
 NA
71mm-100mm
Min 355Mpa
490-620Mpa
21%
-60
 NA
The min impact energy is longitudinal energy

 
 
 
 
Our mill FH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
To get our competitive quotation, please feel free to contact us.
 
 

Tags: FH36  LR/FH36  LR FH36  FH36 steel  LR FH36 steel  LR/FH36 steel  LR  FH36 steel plate  

0 Comments, 0 Trackbacks