LR AH 55 Chemical composition heat analysis

Element
LR AH 55 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
 
 
 
 
LR AH 55 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
LR AH 55
8-260
550
670-830
16
37J

Note: the impact energy under less 150mm thickness
 
 
 