2011年11月8日 by admin

LR DH 55 STEEL PLATE

 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
 
For more information in LR DH 55 steel grade, please refer to the following:

 
 
 
LR DH 55 Chemical composition heat analysis

Element
LR DH 55 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
         
 
 
 
LR DH 55 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
LR DH 55
8-260
550
670-830
16
37J