New Products /back


S460QL steel Grade

2011年3月11日 by admin

 

S460Q/QL/QL1 steel plate from Gangsteel
 
Adopt standard: S460Q EN 10025-6
Sell steel grade: S460Q steel plate, S460QL steel plate, S460QL1 steel plate
 
S460Q/QL/QL1 Steel Grade
 
S460Q S460QL and S460QL1 high yield strength structural steels grade in the quenched and tempered and
S460Q/QL/QL1 steel plate could be used in Mechanical Engineering,suspension arm and others parts in machine.

 
If you need more yield strength, you could choose our others grade in S690Q, S890Q or S960Q
 
Gangsteel sell S460Q S460QL and S460QL1EN 10025-6 steel plates directly from our mill. Gangsteel are special field of exporting steel plate on base of large relation with our mill in China.
 
.About S460Q/QL/QL1 detail information, please consult technical date in following.
 
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
N %
B %
Cr %
 
S460Q
 
0.200
0.800
1.700
0.030
0.017
0.015
0.005
1.500
Cu %
Mo %
Nb %
Ni %
Ti %
V %
Zr %
 
0.500
0.700
0.060
2.000
0.050
0.120
0.150
 

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S460Q
8mm-50mm
Min 460Mpa
550-720Mpa
17%
-20
Min 30J
51mm-100mm
Min 440Mpa
550-720Mpa
17%
-20
Min 30J
101mm-150mm
Min 400Mpa
500-670Mpa
17%
-20
Min 30J

 
 