SA516 Gr.65 steel is a carbon pressure vessel steel grade for moderate and lower temperature service for a variety of applications in the Petrochemical, Chemical, Oil & Gas Industries
 
SA516 Gr.65 usual request normalized if thickness above 40mm, if not, Gangsteel usual delivery in hot rolled or control rolled station. SA516 Gr.65+N or SA516 gr.65N mean that steel grade must be normalized in any thickness.
 
Compare with the SA516 Grade 70, the SA516 Gr.65 steel grade have lower property in tensile and yield strength. Gangsteel also supply the Ultrasonic test in thickness in A435/A435M, A577/577M and A578/A578M to promise the perfect quality in long cooperation.
 
SA516 Gr.65 steel grade is a advantage Gangsteel company, we exported the super thickness steel plate max 140mm in SA516 Gr.65 to Singapore in the best quality. the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.
 
About SA516 Gr.65 , please check technical date in following.detail information
 
 
The A 516 Gr.65 Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
SA516 Gr 65
0.24-0.29
0.13-0.45
0.79-1.3
0.035
0.035


The mechanical properties at SA516 Gr.65 steel plate:

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
SA516 Gr.65
6mm-40mm
240Mpa
450-585Mpa
23%
40mm-100mm
240Mpa
450-585Mpa
19%
The min impact energy is longitudinal energy

 
 Related Grade: SA516 Grade 55 | SA516 Grade 60 |SA516 grade 70
 