SA516 Gr.70steel is a carbon pressure vessel steel grade for moderate and lower temperature service.

 

SA516 Gr.70 usual request normalized if thickness above 40mm, if not, Gangsteel usual delivery in hot rolled or control rolled station. A516 Gr.70+N or A516gr70N mean that steel grade must be normalized in any thickness.

 

Compare with the SA516 Gr.60, SA516 Gr.65, and SA516 Gr.55, the SA516 Gr.70 steel grade have better property in tensile and yield strength. Gangsteel also supply the Ultrasonic test in thickness in A435/A435M, A577/577M and A578/A578M to promise the perfect quality in long cooperation.

 

SA516 Gr.70 steel grade is a advantage Gangsteel company, we exported the super thickness steel plate max 135mm in SA516 Gr.70 to Singapore in the best quality. Our leader is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

About SA516 Gr.70 detail informationplease check technical date in following.

 

 

The SA516 Gr.70 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

SA516 Gr.70

0.27-0.31

0.13-0.45

0.79-1.3

0.035

0.035



 

 

 

 

The mechanical properties at A 516 Gr.70 steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA516 Gr.70

6mm-40mm

260Mpa

485-620Mpa

21%

40mm-100mm

260Mpa

485-620Mpa

17%

The min impact energy is longitudinal energy



 

 

 Related Grade: SA516 Grade 60 | SA516 Grade 65 |SA516 grade 55


If you have any need in SA516 Gr.70, please feel free to contact us soon by email or calling. We will reply to you as early as possible.

Tags: SA516 Gr.70  SA516 Grade 70  ASME SA516 Gr.70  HIC SA516 Gr.70  

0 Comments, 0 Trackbacks