SA516 Grade 60steel grades is used in moderate and lower temperature pressure vessels steel because of the steel material chemical composition and the property in welding.

 

For the reason of excellent notch toughness and weld ability of SA516 Grade 60, it sells good to large fabricators service in gas & oil plants.

 

As the largest exported in our mill, Gangsteel also have SA516 Grade 70, SA516 Grade 65, and SA516 Grade 60 steel plate stock list. Gangsteel has long cooperated company in Indonesia boiler factory and endeavored to enlarge our oversea steel market.


Gangsteel promise that we will use our better service, faster delivery time and the best quality to service our customers. Welcome to visit Gangsteel company and our mill in China

 

About SA516 Grade 60 detail informationplease check technical date in following.

 

 

The SA516 Grade 60 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

SA516 Gr 60

0.21-0.27

0.13-0.45

0.55-1.3

0.035

0.035



 

 

 

The mechanical properties at SA516 Grade 60 steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA516 Gr.60

6mm-40mm

220Mpa

415-550Mpa

25%

40mm-100mm

220Mpa

415-550Mpa

21%

The min impact energy is longitudinal energy



 

 

 Related Grade: SA516 Grade 55 | SA516 Grade 65 |SA516 grade 70

 

If you have any need in SA516 Grade 60, please feel free to contact us soon by email or calling. We will reply to you as early as possible.

Tags: SA516 Grade 60  SA516 Gr.60  SA516 Gr.60 steel plate  ASME SA516 Grade 60  HIC SA516 Grade 60  

0 Comments, 0 Trackbacks