New Products /back


ASME SA537 Class 2 steel plate

2013年8月28日 by admin

Adopt standard: ASME SA537

 

Steel plate SA537 CL2 is a quenched and tempered steel material, higher tensile and yield in property comparing with SA537 CL1 and SA537 CL3.


SA537 CL2 steel plate max thickness is 150mm according to standard of SA537/ SA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.

 

Gangsteel supply SA537 CL2 steel material in many years experience. From melting to ingot product, to rolling plate, we have specialized person tracking it for our customers to promise the delivery time and quality in time.


Welcome to visit our mill in China for long steel business cooperation.

 

About SA537 Cl2 detail information,please check technical date in following.

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

Cu %

Ni %

Cr %

Mo %

SA537 CL2

0.240

0.13-0.55

0.64-1.46

0.035

0.035

0.380

0.280

0.290

0.090



 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate:

 Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA537 CL2

8mm-65mm

Min 415Mpa

550-690Mpa

22%

66mm-100mm

Min 380Mpa

515-655Mpa

22%

101mm-150mm

Min 315Mpa

485-620Mpa

20%

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

For more information in quality certificate or inquiry in competitive official quotation, please contact us.

Tags: SA537 CL2  SA537 CL2 steel  SA537 CL2 steel plate  SA537 Class 2  ASME SA537  

0 Comments, 0 Trackbacks