New Products /back


SA537 Class 2,SA537 Class 2 steel,SA537 Class 2 steel plate

2013年8月28日 by admin

Adopt standard: ASME SA537

SA537 Class 2 steel grade
 
Steel plate SA537 Class 2 is a quenched and tempered steel material, higher tensile and yield in property comparing with SA537 CLASS 1 and SA537 Class 3.

SA537 CLASS 2 steel plate max thickness is 150mm according to standard of SA537/ SSA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.
 
Gangsteel supply SA537 Class 2 steel material in many years experience. From melting to ingot product, to rolling plate, we have specialized person tracking it for our customers to promise the delivery time and quality in time.
 
About SA537Class 2 detail information, please check technical date in following.
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
Cu %
Ni %
Cr %
Mo %
SA537 CLASS 2
0.240
0.13-0.55
0.64-1.46
0.035
0.035
0.380
0.280
0.290
0.090

 
The mechanical properties at ambient temperature for quenched and tempered steel plate:

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
SA537CLASS 2
8mm-65mm
Min 415Mpa
550-690Mpa
22%
66mm-100mm
Min 380Mpa
515-655Mpa
22%
101mm-150mm
Min 315Mpa
485-620Mpa
20%

 
Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17
 
For more information in quality certificate or inquiry in competitive official quotation, please contact us.

Tags: SA537 Class 2  SA537 Class 2 steel  SA537 Class 2 steel plate  ASME SA537 Class 2  

0 Comments, 0 Trackbacks