SA537CL2,SA537CL2 steel,SA537CL2 steel plate

2013年8月28日 by admin

Adopt standard: ASME SA537

 
Steel plate SA537CL2 is a quenched and tempered steel material.
 
SA537CL2 has more in tensile and yield in property comparing with SA537CL1 and SA537CL3.

SA537CL2 steel plate max thickness is 150mm according to standard of SA537/ SA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.
 
Gangsteel supply SA537CL2 steel material in many years experience. From melting to ingot product, to rolling plate, we have specialized person tracking it for our customers to promise the delivery time and quality in time.

Welcome to visit our mill in China for long steel business cooperation.
 
About SA537CL2 detail information, please check technical date in following.
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
Cu %
Ni %
Cr %
Mo %
SA537CL2
0.240
0.13-0.55
0.64-1.46
0.035
0.035
0.380
0.280
0.290
0.090

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
SA537CL2
8mm-65mm
Min 415Mpa
550-690Mpa
22%
66mm-100mm
Min 380Mpa
515-655Mpa
22%
101mm-150mm
Min 315Mpa
485-620Mpa
20%

 Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17
 
For more information in quality certificate or inquiry in competitive official quotation, please contact us.
 

Tags: SA537CL2  Ss537 Cl.2  SA537CL2 steel  SA537CL2 steel plate  

0 Comments, 0 Trackbacks