Adopt standard: ASME SA537

 
SA537Cl1 steel plate is heat treated, Carbon- Manganese- Silicon Pressure Vessel plates.
 
The maximum thickness of plates furnished under100mm according to SA537 standard. But if you need larger thickness in SA537Cl1, our mill also has a ability to produce for you because width and thickness plate are our advantage.
 
SA537Cl1 steel plates shall be normalized in all of thickness. SA537 steel material usual be serviced the Gas, Petrochemical and Oil industry. If you need more yield and tensile grade, you could choose steel grade SA537 Cl2.
 
Gangsteel supply SA537Cl1 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.1 or 3.2.
About SA537Cl1 detail information, please check technical date in following.
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
Cu %
Ni %
SA537Cl1
0.240
0.13-0.55
0.64-1.46
0.035
0.035
0.380
0.280

 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation (%)
SA537Cl1
8mm-65mm
Min 345Mpa
485-620Mpa
22%
66mm-100mm
Min 310Mpa
450-585Mpa
22%
101mm-150mm
A
A
A
A mean that product is not available in this size range

Our mill SA537Cl1 always be exported to Jordan and the middle east city for tank and vessel.
 