New Products /back


ASME SA537 Class 3 steel plate

2013年8月28日 by admin

Steel plate SA537 Cl3 is a quenched and tempered steel material, the same with SA537 Cl2 in heat treatment.

 

Although the SA537 Cl3 only yields strength lowers than A573 Cl2, the two grades have a little different in price. A 537 cl3 quenched and tempered temperature is 620, and SA537 cl2 is 595


SA537 Cl3 steel plate max thickness is 150mm according to standard of A537/SA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.

 

Gangsteel supplies SA537 Cl3 on the base of customer’s request. We could do S1, S2, S3, S4.1, S5, S6, S7, S8, S11, S12,S14 AND S17 supplementary requirements.

 

About SA537 Cl3 detail information, please check technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

Cu %

Ni %

Cr %

SA537 Cl3

0.240

0.13-0.55

0.64-1.46

0.035

0.035

0.380

0.280

0.290



 

 The mechanical properties at ambient temperature for quenched and tempered steel plate:

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA537 Cl3

8mm-65mm

Min 380Mpa

550-690Mpa

22%

66mm-100mm

Min 345Mpa

515-655Mpa

22%

101mm-150mm

Min 275Mpa

485-620Mpa

20%

 

For more information SA537 Cl3 in quality certificate or inquiry in competitive official quotation, please contact us.

Tags: SA537 Cl3  SA537 Cl3 steel  SA537 Cl3 steel plate  SA537 Cl.3 supplier  ASTM A537 Class 3  

0 Comments, 0 Trackbacks